Hello. Sign In
Standards Store
Look Inside

AASHTO M 203M/M 203

2012 Edition, January 1, 2012

Complete Document

Standard Specification for Steel Strand, Uncoated Seven-Wire for Concrete Reinforcement

Includes all amendments and changes through Reaffirmation Notice , 2016


View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

EN
Additional Comments:
ONLY AVAILABLE IN ELECTRONIC FORMAT
Format
Details
Price (USD)
PDF
Single User
$42.00
Add to Cart

People Also Bought These:

ASTM A703/A703M
ASTM A781/A781M
API RP 9B
API SPEC Q1

Product Details:


Description / Abstract:

This specification covers two types and two grades of steel strand, uncoated seven-wire for use in pretensioned and post-tensioned prestressed concrete construction. The two types of strand are low-relaxation and stress-relieved (normal-relaxation). Low-relaxation strand shall be regarded as the standard type. Stress-relieved (normal-relaxation) strand will not be furnished unless specifically ordered or by arrangement between purchaser and supplier. Grade 1725 [250] and Grade 1860 [270] have minimum ultimate strengths of 1725 MPa [250 ksi] and 1860 MPa [270 ksi], respectively, based on the nominal area of the strand.

The values stated in either inch-pound units or SI units are to be regarded as standard. Within the text, the inch-pound units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.

The supplementary requirements in S1 shall be specified for 15.24-mm- [0.600-in.-] diameter uncoated seven-wire steel strand if needed for applications in prestressed ground anchors.