Hello. Sign In
Standards Store

ASD-STAN PREN 4826

Revision P1, March 31, 2013

Complete Document

Aerospace series Zinc-Nickel (12-16 % Ni) plating of steels with specified tensile strength Less than or equal to 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners



Detail Summary

Active, Most Current

EN
Format
Details
Price (USD)
PDF
Single User
$86.00
Print
In Stock
$86.00
PDF + Print
In Stock
$120.40 You save 30%
Add to Cart

People Also Bought These:

NAS410
NASM1312-11
NAS4003
AIAG IATF 16949

Product Details:

  • Revision: Revision P1, March 31, 2013
  • Published Date: March 31, 2013
  • Status: Active, Most Current
  • Document Language: English
  • Published By: ASD-STAN (Formerly AECMA-STAN) (ASD-STAN)
  • Page Count: 13
  • ANSI Approved: No
  • DoD Adopted: No

Description / Abstract:

This standard specifies the plating of a Zinc-Nickel (12 % to 16 %) alloy on mechanical parts and fasteners in steels (UTS ≤ 1 450 MPa), stainless steels (UTS ≤ 1 450 MPa), copper alloys and aluminium alloys (not applicable for electrical components), as well as the passivation and lubricant finishing that can be associated to them. The Zinc-Nickel process is an electrolytic plating process under controlled current allowing to deposit a Zinc-Nickel layer from, most often, an alkaline electrolyte. Alkaline Zinc-Nickel is only considered in this standard.