Hello. Sign In
Standards Store

ASTM D3217/D3217M

2015 Edition, February 1, 2015

Complete Document

Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

Price (USD)
Single User
In Stock
PDF + Print
In Stock
$78.20 You save 15%
Add to Cart

Product Details:

  • Revision: 2015 Edition, February 1, 2015
  • Published Date: February 1, 2015
  • Status: Active, Most Current
  • Document Language: English
  • Published By: ASTM International (ASTM)
  • Page Count: 5
  • ANSI Approved: No
  • DoD Adopted: No

Description / Abstract:

These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot.

Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included.

Elongation in loop or knot tests has no known significance, and is usually not recorded.

The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot.

The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.