1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot.

1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included.

1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded.

1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot.

1.5 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system are not necessarily exact equivalents; therefore, to ensure conformance with the standard, each system shall be used independently of the other, and values from the two systems shall not be combined.

1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.7 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

 

Document History

  1. ASTM D3217/D3217M-20

    👀currently
    viewing


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Most Recent
  2. ASTM D3217/D3217M-15


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Historical Version
  3. ASTM D3217/D3217M-13


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Historical Version
  4. ASTM D3217-07


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Historical Version
  5. ASTM D3217-01a


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Historical Version
  6. ASTM D3217-01


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Historical Version
  7. ASTM D3217-95


    Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations

    • Historical Version