DELAY COMPOSITION, TUNGSTEN-FLUOROCARBON COPOLYMER
Includes all amendments and changes through Interim Notice 1, July 10, 1999
Additional Comments: INACTIVE FOR NEW DESIGN AFTER 7/10/99
PDF :
$31.00 USD
In Stock
Print  :
$34.00 USD
In Stock
Print + PDF :
$45.50 USD
You save 30%
In Stock
This specification covers one type of Tungsten-Fluorocarbon copolymer delay composition.

This type of delay composition shall be of three classes depending upon the burning time ranges, as follows:

Class I 2.5 to 7.5 sec/in at 24 ± 4°C.

Class II 7.5 to 12.5 sec/in at 24 ± 4°C.

Class III 12.5 to 32.5 sec/in at 24 ± 4°C.