SAE AMS2451/2 Revision A, June 1, 2006
Complete Document
Active, Most Current
Plating, Brush, Nickel Low Stress, Hard Deposit
Includes all amendments and changes through Reaffirmation Notice , April 2011
Page Count:2
$74.00 USD
In Stock
Print  :
$74.00 USD
In Stock
AIA/NAS Aerospace Standards

This specification covers the requirements and process controls for brush plating of hard, low stress nickel by electrodeposition.


This process has been used typically to improve wear resistance and to repair damaged, worn, or mismachined parts in applications requiring hardness, fatigue resistance, and service at temperatures up to 450 °F (232 °C) but usage is not limited to such applications.