(R) Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H900) 180 ksi (1241 MPa) Tensile Strength (17-4)

Includes all amendments and changes through Reaffirmation Notice , October 2013


View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

EN
Format
Details
Price (USD)
PDF
Single User
$78.00
Print
In Stock
$78.00
Add to Cart

People Also Bought These:

ASTM A370
ASTM E18
SAE AS9101
SAE AMS5643

Product Details:

  • Revision: Revision F, February 1, 2007
  • Published Date: October 2013
  • Status: Active, Most Current
  • Document Language: English
  • Published By: SAE International (SAE)
  • Page Count: 11
  • ANSI Approved: No
  • DoD Adopted: Yes

Description / Abstract:

Form

This specification covers a corrosion-resistant steel in the form of investment castings.

Application

These castings have been used typically for parts requiring good corrosion resistance and strength up to 600 °F (316 °C), but usage is not limited to such applications (See 8.4).

Certain processing procedures and service conditions may cause these castings to become subject to stresscorrosion cracking; ARP1110 recommends practices to minimize such conditions.