Revision E, May 1, 2007

Complete Document

Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb(Nb) - 0.90Ti - 0.60Al - 18Fe Vacuum Melted Homogenization and Solution Heat Treated

Includes all amendments and changes through Reaffirmation Notice , October 2012


View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

EN
Format
Details
Price (USD)
PDF
Single User
$76.00
Print
In Stock
$76.00
Add to Cart

People Also Bought These:

ASTM E1417/E1417M
ASTM E18
AWS A2.4
AWS D17.1/D17.1M

Product Details:

  • Revision: Revision E, May 1, 2007
  • Published Date: October 2012
  • Status: Active, Most Current
  • Document Language: English
  • Published By: SAE International (SAE)
  • Page Count: 11
  • ANSI Approved: No
  • DoD Adopted: Yes

Description / Abstract:

Form

This specification covers a corrosion and heat-resistant nickel alloy in the form of investment castings.

Application

These casting have been used typically for structural parts requiring strength up to 1300 °F (704 °C) and oxidation resistance up to 1800 °F (982 °C ), but usage is not limit to such applications.

Classification Casting conforming to this specification is classified as follows:

Class 1 Trace element limits conforming to AMS 2280-1

Class 2 Trace element limits conforming to AMS 2280-2

Class 3 Trace element limits do not apply

Casting shall conform to Class 3 unless Class 1 or Class 2 is specification by purchaser.