SAE AMS5605

Revision F, August 1, 2013

Complete Document

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated



View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

EN
Format
Details
Price (USD)
PDF
Single User
$78.00
Print
In Stock
$78.00
Add to Cart

Product Details:

  • Revision: Revision F, August 1, 2013
  • Published Date: August 2013
  • Status: Active, Most Current
  • Document Language: English
  • Published By: SAE International (SAE)
  • Page Count: 7
  • ANSI Approved: No
  • DoD Adopted: No

Description / Abstract:

Form

This specification covers a corrosion and heat-resistant nickel alloy in the form of sheet, strip, and plate 1.00 inch (25.4 mm) and under in nominal thickness.

Application

These products have been used typically for parts requiring good machinability and high strength at room and cryogenic temperatures and for short-time use up to 1000 °F (538 °C), particularly for those parts which are formed or welded and then heat treated to develop required properties, but usage is not limited to such applications.
AIA/NAS Aerospace Standards