Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800 °F (982 °C) Solution Heat Treated, Precipitation-Hardenable



View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

EN
Format
Details
Price (USD)
PDF
Single User
$78.00
Print
In Stock
$78.00
Add to Cart

People Also Bought These:

ASTM E18
ASTM A370
ASTM A193/A193M
SAE AMS4928

Product Details:

  • Revision: Revision G, August 2018
  • Published Date: August 2018
  • Status: Active, Most Current
  • Document Language: English
  • Published By: SAE International (SAE)
  • Page Count: 7
  • ANSI Approved: No
  • DoD Adopted: No

Description / Abstract:

Form

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, and flash-welded rings under 4.00 inches (101.6 mm) in nominal thickness or diameter, and stock of any size for forging, flash-welded rings, or heading (see 8.6).

Application

These products have been used typically for parts requiring high strength in the range 800 to 1100 °F (427 to 593 °C), particularly those parts which are formed or welded and then precipitation heat treated to develop required properties, but usage is not limited to such applications.