Hello. Sign In
Standards Store

SAE AMS5853

Revision C, June 1, 2006

Complete Document

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength

Includes all amendments and changes through Reaffirmation Notice , April 2012


View Abstract
Product Details
Document History

Detail Summary

Active, Most Current

EN
Format
Details
Price (USD)
PDF
Single User
$76.00
Print
In Stock
$76.00
Add to Cart

People Also Bought These:

ASME B46.1
SAE AMS-H-6875
SAE AMS2700
SAE AMS5731

Product Details:

  • Revision: Revision C, June 1, 2006
  • Published Date: April 2012
  • Status: Active, Most Current
  • Document Language: English
  • Published By: SAE International (SAE)
  • Page Count: 5
  • ANSI Approved: No
  • DoD Adopted: No

Description / Abstract:

Form

This specification covers a corrosion and heat-resistant steel in the form of work-strengthened bars and wire, 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides.

Application

These products have been used typically for parts, such as fasteners, requiring room-temperature minimum tensile strength of 160 ksi (1103 MPa) after precipitation heat treatment for use up to 1000 °F (538 °C) and having oxidation resistance up to 1200 °F (649 °C), but usage is not limited to such applications.

AIA/NAS Aerospace Standards